Home » Product List » Alloy » Rod / Wire electrodes for Aluminium (4043)
Product Details
Rod / Wire electrodes for Aluminium (4043)
| Productivity: | 50, 000 tons/year |
|---|---|
| Unit Price/Payment: | TT, L/C |
| HS Code: | 72292000 |
| Trademark: | changjiang |
| Origin: | china |
| Min. Order: | 20T |
| Product Type: | Tools and Hardware |
Rod/ Wire electrodes for Aluminium
Performance & Usage:
This is a kind of pure aluminium welding wire with the aluminum more than 99.5%. It has advantages ranges over good anti-corrosiveness, well electrical conductivity and processiveness. And it also is a kind of best choice for color-match after anodic process. Recommended type: Aluminium alloy 1000
Product usage: Engine, electric power, chemistry, food, etc.
Shielding gas: I1, I2, I3(Argon, Helium or Argon/Helium-mixtures)
Dimensions ¦µ:
MIG-/MIG-wires(mm): 0.8; 0.9; 1.0; 1.2; 1.6; 2.0; 2.4
WIG-/TIG-rods(mm): 1.6; 2.0; 2.4; 3.2; 4.0; 5.0; 6.0
Wire packagings: (Spools): S100/0.5kg(1lb); S200/2kg; S3006kg-7kg(16lb); S360/20kg
Rod packagings: (Boxes)5/10kg: Length 1.000mm
Notice of usage and storage:
1. You can do welding directly in effect without any processing before welding after opening the box of products, The products will be in effect more than two years on condition they are of good packing in seal.
2. The products should be put to the place where is of aeration and dryness and away from the medium of acid\alkali\oil and so on.
3. The products should be avoided of crack and damp during delivery so as to avoid destroying the welding spools and impacting the quality of welding wires.
4. We suggest you to put some dust-proof on the surface of wires after the packages are moved from the products.
5. We suggest you to do some processing to the surface of the wires before welding when you use the wires out of storage life.
6. The arc welding may hurt your eyes during welding. Please protect your eyes.