Alloy cored wire is always applied in the method of feeding-wire, depending on the diameter of cored wire alloy and wire material melting point, it can set the speed. And it is made vertically by feeding wire machine, smoothly mixing the liquid of steel and iron, In ideal and depth steel-making situation, it would be happened physical and chemical reaction, avoided adding the reaction of elements to air and molten slag, improves the yield degree rate of the element yield, achieve the aim of refined melting, changing the precision component height, alloying, and the improvement of the composition, it has the remarkable usage to increase the quality of melting steel and iron, decrease the cost of the melting process, and has a significant the cast iron and steel economical benefit.
No
|
Name
|
Chemical composition ( % )
|
Wire diameter (mm)
|
Belt Iron thickness (mm)
|
Belt iron
weight (g/m)
|
Cored powder weight (g/m)
|
Uniformity
degree (%)
|
1
|
Cored wire SiCa
|
Si55Ca30
|
13.0
|
0.35
|
145
|
230
|
2.5-5
|
2
|
Cored wire AlCa
|
Ca26-30AI3-24
|
13.0
|
0.35
|
145
|
210
|
2.5-5
|
3
|
Cored wire CaFe
|
Ca28-35
|
13.0
|
0.35
|
145
|
240
|
2.5-5
|
4
|
Cored wire SiCaBa
|
Si55Ca15Ba15
|
13.0
|
0.35
|
145
|
220
|
2.5-5
|
5
|
Cored wire
SiAlBa
|
Si35-40Al 12-16 Ba9-15
|
13.0
|
0.35
|
145
|
215
|
2.5-5
|
6
|
cored wire SiCaAl
|
Si30-45Ca9-14
|
13.0
|
0.35
|
145
|
225
|
2.5-5
|
7
|
Cored wire
ReSi
|
Mg5-10Re1-5
Ba1-3Ca2-4Si30-50
|
13.0
|
0.35
|
145
|
230
|
2.5-5
|
8
|
Cored wire
TiFe
|
Ti30
|
13.0
|
0.35
|
145
|
510
|
2.5-5
|
9
|
Cored wire
Increasing Ca
|
C98s<0.5
|
13.0
|
0.35
|
145
|
150
|
2.5-8
|
10
|
Cored wire
High Mg
|
Mg30-32Si40-44
Ca1.5-20Ba1.5-20Re1.5-2.0
|
13.0
|
0.35
|
145
|
|
2.5-5
|