Specification |
Application: Industrial;
Standard: JIS, GB, DIN, ASTM, AISI;
Purity: Ni 60%, Cr 15%;
Alloy: Alloy;
Type: Nickel Wire;
Powder: Not Powder;
Surface: Bright;
Condition: Annealed;
Equal to: Nikrothal 60;
Resistivity: 1.14 Ohm mm2/M;
Density(g/cm3): 8.2;
Size: 24~32 Gauge;
Grade:  Cr15ni60;
Chemical Composition: Cr 15~18% Ni 55~61% Fe Rest;
Max. Continuous Service Temp. of Element: 1150;
|
Application: Aviation, Electronics, Industrial, Medical, Chemical;
Standard: JIS, GB, DIN, BS, ASTM, AISI;
Purity: 24-27;
Alloy: Alloy;
Type: Nickel Pipe;
Powder: Not Powder;
Grade: Nickel, Chromium, Molybdenum, Iron and Titanium;
Model Number: Gh3030 Gh2132 Gh3039 Gh3128 Gh3044;
Material: Gh2747 Pipe;
Density: 8.3G/Cm3;
Melting: 1300-1390°c;
Surface: Bright;
Forging Heating Temperature: 1170~1190ºC;
Elongation: 3.5;
Process Method: Cold Drawn;
|
Application: Aviation, Electronics, Industrial, Medical, Chemical;
Standard: JIS, GB, DIN, BS, ASTM, AISI;
Alloy: Alloy;
Type: Nickel Pipe;
Powder: Not Powder;
Grade: Nickel, Chromium, Molybdenum, Iron and Titanium;
Model Number: Gh3030 Gh2132 Gh3039 Gh3128 Gh3044;
Material: Gh2747 Pipe;
Density: 8.3G/Cm3;
Melting: 1300-1390°c;
Surface: Bright;
Forging Heating Temperature: 1170~1190ºC;
Elongation: 3.5;
Process Method: Cold Drawn;
|
Application: Aviation, Electronics, Industrial, Medical, Chemical;
Standard: JIS, GB, DIN, BS, ASTM, AISI;
Alloy: Alloy;
Type: Nickel Pipe;
Powder: Not Powder;
Grade: Nickel, Chromium, Molybdenum, Iron and Titanium;
Model Number: Gh3030 Gh2132 Gh3039 Gh3128 Gh3044;
Material: Gh2747 Pipe;
Density: 8.3G/Cm3;
Melting: 1300-1390°c;
Surface: Bright;
Forging Heating Temperature: 1170~1190ºC;
Elongation: 3.5;
Process Method: Cold Drawn;
|
Application: Aviation, Electronics, Industrial, Medical, Chemical;
Standard: JIS, GB, DIN, BS, ASTM, AISI;
Purity: 24-27;
Alloy: Alloy;
Type: Nickel Pipe;
Powder: Not Powder;
Grade: Nickel, Chromium, Molybdenum, Iron and Titanium;
Model Number: Gh3030 Gh2132 Gh3039 Gh3128 Gh3044;
Material: Gh2747 Pipe;
Density: 8.3G/Cm3;
Melting: 1300-1390°c;
Surface: Bright;
Forging Heating Temperature: 1170~1190ºC;
Elongation: 3.5;
Process Method: Cold Drawn;
|