Specification |
Material: Steel;
Content: 75% ~ 80%;
Usage: Grind;
Processing Type: Rolling Type;
Size: 10-165mm;
Color: Brown;
Customized: Customized;
No Breakage: Tough Surface to Tough Core;
Good Wear Rate: for Sag Mills and Ball Mills;
Good Performance: High Quality;
High Heat Treatment Technology: for Zinc Mines;
|
Material: Alloy Steel, Carbon Steel, Round Steel, Steel Iron;
Content: >90%;
Usage: Construction, Machinery, Chemical, Grind, Cement,Mine,Power Plant, Quartz / Silicon Sand Fac;
Processing Type: Forging,Hot Rolling;
Size: Middle;
Color: Black;
Customized: Customized;
Product Name: Forged Steel Ball;
Service: Customized &Free Samples;
Heat Treatment: Quenching+Tempering;
Steel Ball Hardness: 60-65HRC;
Breakage Rate: <1%;
Impact Toughness: >12ak.J/Cm^2;
Other Application: Power Plant, Quartz / Silicon Sand Factory;
|
Material: Steel;
Content: >90%;
Usage: Construction, Machinery, Chemical, Grind, Ball Mill, Mining,Cement Plant,Sag Mill;
Processing Type: Forging/Rolling;
Size: Customized;
Color: Black;
Customized: Customized;
Product Name: Forged Grinding Steel Ball;
Application: Ball Mill,Sag Mill,Mineral Process;
Service: Free Samples;
Hardness: 55-66 HRC;
Impact Toughness: >12 Ak.J/C M^2;
Loss Roundness Rate: <1%;
Breakage Rate: <1%;
Heat Treatment: Tempering & Quenching;
|
Material: Steel;
Content: >90%;
Usage: Construction, Machinery, Chemical, Grind, Ball Mill, Mining,Cement Plant,Sag Mill;
Processing Type: Forging/Rolling;
Size: Customized;
Color: Black;
Customized: Customized;
Product Name: Forged Grinding Steel Ball;
Application: Ball Mill,Sag Mill,Mineral Process;
Service: Free Samples;
Hardness: 55-66 HRC;
Impact Toughness: >12 Ak.J/C M^2;
Loss Roundness Rate: <1%;
Breakage Rate: <1%;
Heat Treatment: Tempering & Quenching;
|
Material: Stainless Steel;
Content: >90%;
Usage: Construction, Chemical, Grind, Mining, Cement Plant;
Processing Type: Forged & Cast;
Size: Middle;
Color: Brown;
Customized: Customized;
Product Name: Grinding Steel Balls;
Process: Forged, Hot Rolled;
Service: Free Samples;
Heat Treatment: Quenching + Tempering;
Hardness: 50-65HRC;
Breakage Rate: <1%;
Impact Toughness: >12ak.J/Cm^2;
|