Specification |
Standard: DIN, GB;
Material: Metal;
|
After-sales Service: Onsite Training, Onsite Installation;
Warranty: 3 Year;
Standard: GB;
Material: Metal;
Thickness Range: 0.8-8mm;
Name: Spc Floor Board Mould;
G.W: 10kg;
Delivery Date: 15days;
|
Standard: DIN, ASTM, GOST, GB, JIS, ANSI, ISO;
Technics: Milling-Drilling-Grinding-Polishing;
Material: Tool Steel, Structural & Engineering Steel etc.;
Base Material: 1.8509, 1.8550, 1.8519, 4140, 5140, 45;
Surface Treatment: Bimetallic, Nitriding, Through-Hardened, Chrome-Pl;
Hardness for Nitriding: >Hv900;
Hardness for Bimetallic: HRC50~70 Depending on Different Alloys;
Thickness of Nitriding Layer: 0.4~0.7mm;
Thickness of Bimetallic: 1.5~3.0mm Depending on Different Alloy Coating;
Application: Extruder;
|
Standard: DIN, ASTM, GOST, GB, JIS, ANSI, ISO;
Technics: Milling-Drilling-Grinding-Polishing;
Material: Tool Steel, Structural & Engineering Steel etc.;
Base Material: 1.8509, 1.8550, 1.8519, 4140, 5140, 45;
Surface Treatment: Bimetallic, Nitriding, Through-Hardened, Chrome-Pl;
Hardness for Nitriding: >Hv900;
Hardness for Bimetallic: HRC50~70 Depending on Different Alloys;
Thickness of Nitriding Layer: 0.4~0.7mm;
Thickness of Bimetallic: 1.5~3.0mm Depending on Different Alloy Coating;
Application: Extruder;
|
Standard: DIN, ASTM, GOST, GB, JIS, ANSI, ISO;
Technics: Milling-Drilling-Grinding-Polishing;
Material: Tool Steel, Structural & Engineering Steel etc.;
Base Material: 1.8509, 1.8550, 1.8519, 4140, 5140, 45;
Surface Treatment: Bimetallic, Nitriding, Through-Hardened, Chrome-Pl;
Hardness for Nitriding: >Hv900;
Hardness for Bimetallic: HRC50~70 Depending on Different Alloys;
Thickness of Nitriding Layer: 0.4~0.7mm;
Thickness of Bimetallic: 1.5~3.0mm Depending on Different Alloy Coating;
Alloy Type: Ni60, Colmonoy 56, Colmonoy 83, Tungsten Alloy;
Application: Extrusion Machines;
|