Specification |
Application: Grinding, Wire Cutting, Refractory, Buffering;
Raw Material: Silica Sand;
Sic Content: 98.5%;
Colour: Black and Green;
Usage: Grinding, Polishing, Sandblasting;
Abrasive Grain Sizes: F12-F1200, P12-P2500;
Hardness: Mohs 9.5;
Size: According Customer Requirement;
Other Name: Silicon Carbide Powder;
Shape: Granule, Lump.Powder, Briquette;
Sample: Free;
Grade: First Grade;
|
After-sales Service: 24;
Color: Black;
Application: Refractory, Metallurgy, Ceramic, Casting;
Material: Silicon Carbide;
Shape: Lump,Granule and Powder;
Refractoriness (ºC): 1770< Refractoriness< 2000;
Type: Refractory Material;
Relative Density: 3.2 Mg/Cm3;
Raw Material: Petroleum Coke and Silica Sand;
Standard: GB JIS Oct;
Other Names: Carborundum Block/Sic Grit/Sand/Powder;
|
After-sales Service: 7-24h Online Service;
Color: Black;
Application: Refractory, Metallurgy, Chemical, Ceramic, Casting;
Shape: Powder, Grit;
Material: Silicon Carbide (Sic);
Refractoriness (Degree): 1770°< Refractoriness< 2000°;
Product Name: Refractory Silicon Carbide Powder;
Bulk Density: 1.2-1.6 g/cm3;
Ture Density: 3.2-3.45 g/cm3;
Thermal Conductivity: 71-130 W/M.K;
Coefficient of Thermal Expansion: 3.9-4.5 X10-6/ºC;
Working Temperature: 1900ºC;
|
After-sales Service: 7-24h Online Service;
Color: Black;
Application: Refractory, Metallurgy, Chemical, Ceramic, Casting;
Shape: Powder, Grit;
Material: Silicon Carbide (Sic);
Refractoriness (Degree): 1770°< Refractoriness< 2000°;
Product Name: Refractory Silicon Carbide Powder;
Bulk Density: 1.2-1.6 g/cm3;
Ture Density: 3.2-3.45 g/cm3;
Thermal Conductivity: 71-130 W/M.K;
Coefficient of Thermal Expansion: 3.9-4.5 X10-6/ºC;
Working Temperature: 1900ºC;
|
After-sales Service: 7-24h Online Service;
Color: Black;
Application: Refractory, Metallurgy, Chemical, Ceramic, Casting;
Shape: Powder, Grit;
Material: Silicon Carbide (Sic);
Refractoriness (Degree): 1770°< Refractoriness< 2000°;
Product Name: Refractory Silicon Carbide Powder;
Bulk Density: 1.2-1.6 g/cm3;
Ture Density: 3.2-3.45 g/cm3;
Thermal Conductivity: 71-130 W/M.K;
Coefficient of Thermal Expansion: 3.9-4.5 X10-6/ºC;
Working Temperature: 1900ºC;
|