Specification |
Color: Black;
Appearance: Powder;
Main Raw Material: Resin;
Method: Spray;
Level: Finish Coat;
Substrate: Iron;
Components: Resin;
Paint Film Property: Heat-Resisting Paint;
Formation Mechanism: Conversion Type;
Cured Condition: 200ºC/20mins;
|
Color: Customized;
Appearance: Powder;
Main Raw Material: Polyester Resin;
Method: Spray;
Level: Finish Coat;
Substrate: Metal Surface;
Components: Resin, Pigment, Assistant;
Paint Film Property: Conducting Paint;
Formation Mechanism: Conversion Type;
Features: Anti-Corrosion, Temperature Resistance;
Gloss: High Gloss, Low Gloss;
Leat Time: 3-15days;
N.W: 25kg;
Application: Metal Surface;
Curing Condition: 180-200 Degree/8-10 Minutes;
Adhesion: 0 Level;
Pencial Hardness: 1h-2h;
|
CAS No.: 25135-73-3;
Formula: 2h26o10;
Color: Customized;
Appearance: Powder;
Main Raw Material: Epoxy Polyester;
Method: Spray;
Level: Finish Coat;
Substrate: Metal;
Components: Epoxy Polyester;
Formation Mechanism: Conversion Type;
Features: Anti-Corrosion, Temperature Resistance;
Gloss: High Gloss, Low Gloss;
Leat Time: 3-15days;
N.W: 25kg;
Application: Metal Surface;
Curing Condition: 180-200 Degree/8-10 Minutes;
Impact: 50cm.Kg;
Adhesion: 0 Level;
|
Color: Customized;
Appearance: Powder;
Main Raw Material: Polyester Resin;
Method: Spray;
Level: Finish Coat;
Substrate: Metal Surface;
Components: Resin, Pigment, Assistant;
Formation Mechanism: Conversion Type;
Features: Anti-Corrosion, Temperature Resistance;
Gloss: High Gloss, Low Gloss;
Leat Time: 3-15days;
N.W: 25kg;
Application: Metal Surface;
Curing Condition: 180-200 Degree/8-10 Minutes;
Adhesion: 0 Level;
Pencial Hardness: 1h-2h;
|
Color: Customized;
Appearance: Powder;
Main Raw Material: Polyester Resin;
Method: Spray;
Level: Finish Coat;
Substrate: Metal Surface;
Components: Resin, Pigment, Assistant;
Paint Film Property: Conducting Paint;
Formation Mechanism: Conversion Type;
Features: Anti-Corrosion, Temperature Resistance;
Gloss: High Gloss, Low Gloss;
Leat Time: 3-15days;
N.W: 25kg;
Application: Metal Surface;
Curing Condition: 180-200 Degree/8-10 Minutes;
Adhesion: 0 Level;
Pencial Hardness: 1h-2h;
|