Specification |
Casting Form Material: Metal;
Casting Metal: Cast Iron;
Casting Form Usage Count: Disposable;
Surface Treatment: Polishing;
Surface Roughness: Ra0.2;
Coating: Talcum powder;
Machining Tolerance: +/-0.01mm;
Standard: ASTM;
Name: Knife Edge;
Size: HK1 203-16,HK1 203-25, HK2 203-16, HK3 203-28,etc;
Material: High Chrome Cast Iron&Mild Steel;
Hardness: 63HRC/700bhn;
Tensile Strength: 630MPa Min;
Shearing Strength: 250MPa Min;
Micro-Structure: Carbide+Martensite+Retained Austenite;
Application: Sugar Mill;
Fuction: Crushing, Shredding;
Advatage: Excellent Wear Resistance;
|
Casting Method: Investment Casting/Lost Wax Casting;
Casting Form Material: Wax/Metal/Sand;
Casting Metal: Iron/Cast Steel/Aluminum/Ss etc.;
Casting Form Usage Count: Permanent;
Surface Treatment: Sand Blast/Powder Coating/Electroplating/Polishing;
Surface Roughness: Ra12.5;
Coating: Powder Coating;
Machining Tolerance: +/-0.01mm;
Standard: ASTM/AISI/BS/JIS/GB;
|
Casting Method: Investment Casting/Lost Wax Casting/Gravitycasting;
Casting Form Material: Wax/Metal;
Casting Metal: Aluminum/Cast Iron/Steel;
Casting Form Usage Count: Permanent;
Surface Treatment: Sand Blast/Powder Coating/Electroplating/Polishing;
Surface Roughness: Ra12.5;
Coating: N/A;
Machining Tolerance: +/-0.01mm;
Standard: ASTM;
Factory Location: Ningbo;
Drawing Format: Dwg/Stl/STP/Pdf etc.;
Secondary Service: Heat Treatment/Surface Treatment/Custom Package;
|
Casting Method: Investment Casting/Lost Wax Casting;
Casting Form Material: Wax;
Casting Metal: Iron/Cast Steel/Aluminum/Ss etc.;
Casting Form Usage Count: Permanent;
Surface Treatment: Polishing;
Surface Roughness: Ra12.5;
Coating: N/a;
Machining Tolerance: +/-0.01mm;
Standard: ASTM;
|
Surface Roughness: Min Ra0.8;
Standard: DIN Js ASTM;
Raw Material: CF-3m,Zgcr22ni14,AISI410,Dch23,316L,317L;
Machine: Centrifugal Casting;
Processing: Casting--Machining--Welding;
Application: Continuous Galvanizing Line;
Max Manufacture Ability: 5000t/Year;
|