Specification |
CAS No.: WBPFF;
Color: Customizable;
Appearance: Liquid;
Main Raw Material: Polyurethane;
Method: Brush;
Level: Finish Coat;
Drying Method: Air Drying;
Substrate: Concrete;
Components: Film Forming Matter;
Formation Mechanism: Conversion Type;
Item Name: Water Base Polyurethane Floor;
Drying Time: Surface Drying 1h;
Pencil Hardness: Greater Than or Equal to 2h;
Wear Resistance(750g/500r): Less Than or Equal to 0.02;
Bond Strength: Greater Than or Equal to 2 MPa;
Abhesive (Cross Cut Method): Less Than or Equal to 0;
Impact Resistance: Adopt;
Slip Resistance: Greater Than or Equal to 0.60;
Paint Properties: High Strengh,Abrasion Resistant,Wear Resistant;
Paint Properties More: UV Resistant,High Traffic,Impact Resistant,Chemica;
|
Color: Ral;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Drying Method: Drying;
Substrate: Steel;
Components: Film Forming Matter;
Formation Mechanism: Conversion Type;
Name: Electrostatic Pure Polyester Powder Coating;
Thickness: 60-80um;
Adhesion: 0 Grade;
Hardness: 2h;
Gloss: High Gloss;
Expiration: 12 Months;
Curing: 180 Degree/15mins, 200 Degree/10mins;
Spraying Mode: High Voltage Electrostatic Spraying 40-80kv;
Storage Condition: at About 25 Degree and at Ventilated Indoors;
Spray Ratio: 90%;
Impact Resistance: 50kg/Cm;
Store: in Ventilated, Dry, Temperature < 25ºC;
Bending Test: 5mm;
Anti Resistance: 500h;
Coverage: 8-10 Square Meters Per Kg;
|
Color: Ral;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Substrate: Steel;
Components: Film Forming Matter;
Formation Mechanism: Conversion Type;
Thickness: 60-80um;
Adhesion: 0 Grade;
Hardness: 2h;
Gloss: High Gloss;
Expiration: 12 Months;
Curing: 180 Degree/15mins, 200 Degree/10mins;
Spraying Mode: High Voltage Electrostatic Spraying 40-80kv;
Storage Condition: at About 25 Degree and at Ventilated Indoors;
|
Color: Pink;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Drying Method: Drying;
Substrate: Steel;
Components: Film Forming Matter;
Formation Mechanism: Conversion Type;
Thickness: 60-80um;
Adhesion: 0 Grade;
Hardness: 2h;
Gloss: High Gloss;
Expiration: 12 Months;
Curing: 180 Degree/15mins, 200 Degree/10mins;
Spraying Mode: High Voltage Electrostatic Spraying 40-80kv;
Storage Condition: at About 25 Degree and at Ventilated Indoors;
|
Color: Red;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Drying Method: Air Drying;
Substrate: Steel;
Components: Film Forming Matter;
Formation Mechanism: Conversion Type;
Production Name: Metallic Texture Aluminum Profiles Powder Coating;
Thickness: 60-80um;
Adhesion: 0 Grade;
Hardness: 2h;
Gloss: High Gloss;
Expiration: 12 Months;
Curing: 180 Degree/15mins, 200 Degree/10mins;
Spraying Mode: High Voltage Electrostatic Spraying 40-80kv;
Storage Condition: at About 25 Degree and at Ventilated Indoors;
Ratio: 90%;
|