Specification |
Type: Oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Coil/Strip/Sheet;
Width: 20mm-1250mm;
Material Thickness: 0.23mm-0.3mm/ 0.35mm-0.65mm;
Material Brand: Huaxi Steel, Baosteel, Wisco, Shougang Group;
Material Brand 2: an Steel, Shagang Steel, Xinyu Factory;
Delivery Time: Within 7-15 Days;
Process: Steel Strip or Steel Plate;
Coil Weight: Customized;
Technology: Cold Rolling;
Edge: Slit Edge;
Usage: Power Transformer;
OEM: Offered;
ODM: Offered;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM;
Technique: Cold Rolled;
Shape: EI Lamination;
Thickness: 0.23/0.27/0.3/0.35/0.5mm;
Surface Treatment: Coated;
Packing: RoHS;
Chemical Composition: Silicon Steel;
Material: Cold Rolled Non-Oriented Silicon Steel;
Key Words: Transformer Core;
Size: International Size;
Gap Size on Lamination: No Gap;
Numbers of Holes: 4 or 6 Holes as Per Customers' Demands;
Anneal Treatment: as Per Customers' Demand;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|