Specification |
Type: Oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Coil/Strip/Sheet;
Width: 20mm-1250mm;
Material Thickness: 0.23mm-0.3mm/ 0.35mm-0.65mm;
Delivery Time: Within 7-15 Days;
Process: Steel Strip or Steel Plate;
Material Brand: Sheraxin, Baosteel, Wisco, Shougang Group;
Material Brand 2: an Steel, Shagang Steel, Xinyu Factory;
Coil Weight: Customized;
Technology: Cold Rolling;
Edge: Slit Edge;
Usage: Power Transformer;
OEM: Offered;
ODM: Offered;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;
Weight: 3~8t;
|
Type: Non-oriented Silicon Steel;
Standard: GB, AISI, ASTM, DIN, BS, JIS;
Technique: Cold Rolled;
Shape: Steel Coil;
ID: 508mm;
Nominal Thickness: 0.10mm,0.12mm,0.15mm,0.17mm;
Annealing Temperature: 820±20ºC;
Annealing Time: 1.5 to 2.5 Hours;
The Rate of Heating and Cooling: Rapid Heating or Cooling Should Be Forbidden;
Annealing Atmosphere: Nitriding and Oxidation Atmosphere Must Be Avoided;
Nominal Width: 200~1500mm;