Specification |
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Low Thermal Conductivity;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Powder;
Cao Content %: 3;
Al203 Content (%): 45;
Si02 Content (%: 10%;
Refractoriness (Degree): Common1580< Refractoriness<1770;
Material: Alumina Cement;
Water Required for Casting %: 5-9;
Cao: 2-3%;
Bulk Densityg/Cm3): 2.4-3.0;
Ai203: 45-95%;
Application: Furnace Lining;
Fe203: 1.5-2.4;
|
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Light Weight, Low Thermal Conductivity, Long Time Materials;
Production Process: Extrusion Method;
Refractoriness (℃): 1580< Refractoriness< 1770, 1580< Refractoriness< 1770;
Shape: Brick, Brick;
Type: Refractory Material;
Material: Alumina Block;
Size: Customizable;
Certifiacte: ISO9001, CE, etc;
Bulk Density: 1.45-1.60;
Cold Crushing Strength: 15-20MPa;
Thermal Conductivity: 1.4;
Al2O3: 85-95;
Sio2: 85-99;
|
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Light Weight, Low Thermal Conductivity, Long Time Materials;
Production Process: Extrusion Method;
Refractoriness (℃): 1580< Refractoriness< 1770, 1580< Refractoriness< 1770;
Shape: Brick, Brick;
Type: Refractory Material;
Material: Alumina Block;
Size: Customizable;
Certifiacte: ISO9001, CE, etc;
Bulk Density: 1.45-1.60;
Cold Crushing Strength: 15-20MPa;
Thermal Conductivity: 1.4;
Al2O3: 85-95;
Sio2: 85-99;
|
Feature: Long Time Materials;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Block;
Type: Refractory Material;
Material: Alumina Block;
|
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Light Weight, Low Thermal Conductivity, Long Time Materials;
Production Process: Extrusion Method;
Refractoriness (℃): 1580< Refractoriness< 1770, 1580< Refractoriness< 1770;
Shape: Brick, Brick;
Type: Refractory Material;
Material: Alumina Block;
Size: Customizable;
Certifiacte: ISO9001, CE, etc;
Bulk Density: 1.45-1.60;
Cold Crushing Strength: 15-20MPa;
Thermal Conductivity: 1.4;
Al2O3: 85-95;
Sio2: 85-99;
|