Specification |
Feature: Corrosion Resistance, Good Insulation Performance, Thermal Shock Resistance;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Block;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance, Long Time Materials;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Brick;
Al2O3: at Least 80%;
Zro2: at Least 3%;
Cr2o3: at Least 12%;
Type: Refractory Material;
Material: Corundum and Chromite;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance, Long Time Materials;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Brick;
Al2O3: at Least 80%;
Zro2: at Least 3%;
Cr2o3: at Least 12%;
Type: Refractory Material;
Material: Corundum and Chromite;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance, Long Time Materials;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Brick;
Al2O3: at Least 80%;
Zro2: at Least 3%;
Cr2o3: at Least 12%;
Type: Refractory Material;
Material: Corundum and Chromite;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance, Long Time Materials;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Brick;
Al2O3: at Least 80%;
Zro2: at Least 3%;
Cr2o3: at Least 12%;
Type: Refractory Material;
Material: Corundum and Chromite;
|