Specification |
Materials: Zirconia;
Function: Grinding;
Application: Pigments and Inks and Coatings;
Performance: Low Wear Loss;
Standard: Standard;
Density: 5.0g/cm3;
Zro2: 75%;
Sio2: 20%;
Vickers Hardness: 10gpa;
Wear Volume: 1.5g/Kg.H;
Crushing Strength: 1450n;
Roundness: 95%Min;
|
Materials: Glass Bead Abrasive;
Function: Shot Blasting and Peening,Cleaning,Grinding etc.;
Application: Grinding/Milling/Dispersing Reflective Beads for R;
Performance: High Purity and Good Quality Low Consumption Rate;
Standard: Standard;
Moh's Hardness: 6-7;
Specific Gravity: 2.5g/cm3;
Bulk Density: 1.5g/cm3;
Rockwell Hardness: 46HRC;
Round Rate: ≥80%;
|
Materials: Glass Bead Abrasive;
Function: Shot Blasting and Peening,Cleaning,Grinding etc.;
Application: Grinding/Milling/Dispersing Reflective Beads for R;
Performance: High Purity and Good Quality Low Consumption Rate;
Standard: Standard;
Moh's Hardness: 6-7;
Specific Gravity: 2.5g/cm3;
Bulk Density: 1.5g/cm3;
Rockwell Hardness: 46HRC;
Round Rate: ≥80%;
|
Materials: Glass Bead Abrasive;
Function: Shot Blasting and Peening,Cleaning,Grinding etc.;
Application: Grinding/Milling/Dispersing Reflective Beads for R;
Performance: High Purity and Good Quality Low Consumption Rate;
Standard: Standard;
Moh's Hardness: 6-7;
Specific Gravity: 2.5g/cm3;
Bulk Density: 1.5g/cm3;
Rockwell Hardness: 46HRC;
Round Rate: ≥80%;
|
Materials: Glass Bead Abrasive;
Function: Shot Blasting and Peening,Cleaning,Grinding etc.;
Application: Grinding/Milling/Dispersing Reflective Beads for R;
Performance: High Purity and Good Quality Low Consumption Rate;
Standard: Standard;
Moh's Hardness: 6-7;
Specific Gravity: 2.5g/cm3;
Bulk Density: 1.5g/cm3;
Rockwell Hardness: 46HRC;
Round Rate: ≥80%;
|