Specification |
Casting Method: Directional Crystallization;
Process: Lost Wax Casting;
Molding Technics: Pressure Casting;
Application: Machinery Parts;
Material: Stainless Steel;
Surface Preparation: Polishing;
Surface Roughness: Ra3.2;
Machining Tolerance: +/-0.15mm;
Standard: ANSI;
Castings Material: Stainless Steel , Alloy Steel , Carbon Steel;
Castings Certificate: BV and ISO 9001;
Castings Delivery Time: 30 Days Samples , 30days Batch Production;
Castings Machining: CNC Machining;
Castings Weight: 0.5kg~80 Kg;
Castings: Lost Wax Casting;
Castings Dimension: According to Customer's Drawings;
Testing: Dynamic ,Ut,PT,etc;
|
Casting Method: Directional Crystallization;
Process: Lost Wax Casting;
Molding Technics: Pressure Casting;
Application: Machinery Parts;
Material: Stainless Steel;
Surface Preparation: Sand Blast;
Surface Roughness: Ra1.6;
Machining Tolerance: +/-0.10mm;
Standard: GB;
Weight: 10g-100kg;
Surface Treatment: Burring, Polishing, Shot Blasting, Sandblasting;
Technology: Investment Casting, Lost Wax Casting, Die Casting;
Test Equipment: Coordinate Measuring Machine, X-ray Tester;
Usage: Engineering Parts, Household Appliance;
Mould+Sample Time: 15-25days;
Lead Time: 25-35days;
Inspection: 100%;
|
Casting Method: Directional Crystallization;
Process: Lost Wax Casting;
Molding Technics: Pressure Casting;
Application: Machinery Parts;
Material: Stainless Steel;
Surface Preparation: Sand Blast;
Surface Roughness: Ra1.6;
Machining Tolerance: +/-0.10mm;
Standard: GB;
Weight: 10g-100kg;
Surface Treatment: Burring, Polishing, Shot Blasting, Sandblasting;
Technology: Investment Casting, Lost Wax Casting, Die Casting;
Test Equipment: Coordinate Measuring Machine, X-ray Tester;
Usage: Engineering Parts, Household Appliance;
Mould+Sample Time: 15-25days;
Lead Time: 25-35days;
Inspection: 100%;
|
Casting Method: pressure Crystallization;
Process: Lost Wax Casting;
Molding Technics: Pressure Casting;
Application: Machinery Parts;
Material: Stainless Steel;
Surface Preparation: Sand Blast;
Surface Roughness: Ra1.6;
Machining Tolerance: +/-0.02mm;
Standard: ASTM;
Machining Facility: Mct+CNC;
NDT: Mt/Ut/PT;
Heat Treatment: Normalizing / Qt / Solution Treatment;
Surface Treatment: Electrophoretic Paint;
|
Casting Method: pressure Crystallization;
Process: Lost Wax Casting;
Molding Technics: Pressure Casting;
Application: Machinery Parts;
Material: Stainless Steel;
Surface Preparation: Sand Blast;
Surface Roughness: Ra1.6;
Machining Tolerance: +/-0.02mm;
Standard: ASTM;
Machining Facility: Mct+CNC;
NDT: Mt/Ut/PT;
Heat Treatment: Normalizing / Qt / Solution Treatment;
Surface Treatment: Electrophoretic Paint;
|