Basic Info.
Transport Package
Standard Packaging
Product Description
Note: If you need to customize the shape, size, resistance, etching and scribing, please contact customer service! Commodity informationProduct name: ITO conductive glassSize: 20*20*1.1mmResistance: 3ohm/sqTransmittance: 78%-90%Product packaging: monolithic filmProduct Type: Laboratory SuppliesProduction process: cutting, etching, straight edges, round edges, point corners, drawing lines, digging grooves, opening holes, etc. 50x50x1.1mm 10 Ohm/Sq 10pcs Lab Transparent Conductive Glass Indium Tin Oxide ITO Glass Coated Glass
ITO conductive glassITO conductive glass is made of soda-lime substrate or Penggui substrate glass and coated with a layer of indium tin oxide (commonly known as ITO) film by magnetron sputtering. As a metal compound that does not have good transparent and conductive properties, it has the characteristics of forbidden bandwidth, high light transmittance in the visible spectral region and low resistivity. It is widely used in flat panel display devices, solar cells, special functional window coatings and other optoelectronic devices field.ITO thickness: 0.4mm, 0.5mm, 0.7mm, 0.8mm, 1.0mm, 1.1mm, 1.5mm, 2.0mm, 3.0mm, other thicknesses can be customizedITO resistance: 3-4 ohms, 4-6 ohms, 5-7 ohms/7-10 ohms, 10-15 ohms, 15-20 ohms, 20-30 ohms, 30-40 ohms, 40-60 ohms, 70 -120 ohms, other resistance values can be customized ITO photoelectric performance table |
Specification | Square resistance | Film thickness | Transmittance | Etching time |
3 ohm | 3-4ohm | 380±50nm | ≥80% | ≤400S |
5 ohm | 4-6ohm | 380±50nm | ≥82% | ≤400S |
6 ohm | 5-7ohm | 220±50nm | ≥84% | ≤350S |
7 ohm | 6-8ohm | 200±50nm | ≥84% | ≤300S |
8 ohm | 7-10ohm | 185±50nm | ≥84% | ≤240S |
15 ohm | 10-15ohm | 135±50nm | ≥86% | ≤180S |
20 ohm | 15-20ohm | 95±50nm | ≥87% | ≤140S |
30 ohm | 20-30ohm | 65±50nm | ≥88% | ≤100S |
ITO glass characteristicsAlkali resistance: Alkali resistance means that after immersing in a 10% sodium chloride solution at 60°C for 5 minutes, the change in the square resistance of the ITO layer does not exceed 10%.Acid resistance: Acid resistance means that after immersing in a 25°C, 6% hydrochloric acid solution for 5 minutes, the change in the square resistance of the ITO layer does not exceed 10%Solvent resistant: After 5 minutes in a cleaning solution of 25°C, acetone, absolute ethanol or 100 parts of deionized water plus 3 parts of EC101, the change in the square resistance of the ITO layer does not exceed 10%Adhesion: When the tape is attached to the surface of the film layer and quickly peeled off, the film layer is not damaged; the change of the square resistance of the ITO layer does not exceed 10%Stability: After heating for 30 minutes in the air at 300°C, the square resistance of the ITO conductive film should not exceed 300% of the original square resistance.Conductive glass cleaningDuring the production, packaging and transportation of ITO/FTO conductive glass, the surface of the glass may be contaminated by impurities such as dust, dust and grease. It is necessary to clean ITO and FTO conductive glass before using it. There are many cleaning methods, the most commonly used is ultrasonic cleaning with organic solvents. Grease stained on the glass surface is insoluble in water, but it is soluble in organic solvents such as toluene, acetone, and ethanol. Among them, toluene has the strongest decontamination ability, so first clean with toluene, but toluene cannot remain on the surface of the standard glass. Because toluene is soluble in acetone, it can be cleaned with acetone, which not only cleans out the residual grease, but also dissolves toluene. Similarly, acetone cannot remain on the surface of the glass. As acetone is soluble in ethanol, it can be cleaned with ethanol. Ethanol and water are mutually soluble in any ratio, and then use a large amount of deionized water to dissolve the ethanol, and finally put in anhydrous alcohol to store, and then take it out for use, so that you can wash multiple tablets at once. So generally:Toluene (10-20min) → Acetone (10-15min) → Ethanol (10-20min) → Deionized water (20-30min) in order for ultrasonic cleaning → anhydrous alcohol storage (take it out for long-term storage)
Address:
Yanhuang Science and Technology Park E4-101, No. 333 Kaiyuan Avenue, Luoyang, Henan, China
Business Type:
Manufacturer/Factory
Business Range:
Instruments & Meters
Company Introduction:
It is an enterprise integrating R&D, production and sales of ultra-thin glass. Since its establishment in 2013, with its own exquisite craftsmanship, high-quality products, good procurement channels, honest and prudent service attitude and innovative research spirit, it has become one of the main suppliers in the domestic ultra-thin electronic glass processing and trade industry. In just a few years, it has become a leader in the glass processing trade industry. Focus on customized processing of ultra-thin glass sheets of various materials. B270, BF33, D263T, Corning 2320, K9, quartz, sapphire, Asahi Glass, domestic and other ultra-thin glass sheet processing, drilling and grooving technology, etc.