Specification |
Color: Limited Colors: Grey/Iron Red;
Appearance: Liquid;
Main Raw Material: Epoxy;
Method: Spray/Brush/Roller;
Level: Intermediate Paint;
Drying Method: Air Drying;
Substrate: Steel;
Components: Epoxy Resin, Gray Mica Iron Oxide, Curing Agent;
Formation Mechanism: Conversion Type;
Flash Point: 27ºC;
Weight Ratio: a:B=6:1;
Aging Time: 20ºC, 30min;
Applicable Period: 20ºC, 8h;
Storage Period: 1 Year;
|
Color: Brown/ Grey;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Drying Method: Drying;
Substrate: Steel;
Components: Pigment;
Formation Mechanism: Conversion Type;
Name: Electrostatic Powder Coating;
Effect: Smooth;
Thickness: 60-70um;
Gloss: 80%;
Adhesion: 0 Grade;
Hardness: 2h;
Spray Condition: Electrostatic Spraying;
Curing Condition: 200 Degrees*10 Mins;
Storage Condition: Store in Cool, Dry Place Below 25 Degrees;
Weight: 25kg/Carton;
Expiration: 12 Months;
Application Voltage: 60-90 Kv;
Specific Gravity: 1.2-1.7g Per Cubic Meter;
Ratio: Spray Ratio Is 90%;
Storage Stability: Dry, Clean Room, Temperature < 25ºC;
|
Color: Brown/ Grey;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Drying Method: Drying;
Substrate: Steel;
Components: Pigment;
Formation Mechanism: Conversion Type;
Name: Semi Grey Ral7035 40% Glossy Powder Coating;
Effect: Smooth;
Thickness: 60-70um;
Gloss: 40%;
Adhesion: 0 Grade;
Hardness: 2h;
Spray Condition: Electrostatic Spraying;
Curing Condition: 200 Degrees*10 Mins;
Storage Condition: Store in Cool, Dry Place Below 25 Degrees;
Weight: 25kg/Carton;
Expiration: 12 Months;
Application Voltage: 60-90 Kv;
Specific Gravity: 1.2-1.7g Per Cubic Meter;
Ratio: Spray Ratio Is 90%;
Storage Stability: Dry, Clean Room, Temperature < 25ºC;
|
Color: Blue;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Drying Method: Drying;
Substrate: Steel;
Components: Pigment;
Formation Mechanism: Conversion Type;
Effect: Smooth;
Production Name: Pure Polyester Type Electrostatic Powder Coating;
Thickness: 60-80um;
Adhesion: 0 Grade;
Hardness: 2h;
Gloss: High Gloss;
Expiration: 12 Months;
Curing: 180 Degree/15mins, 200 Degree/10mins;
Spraying Mode: High Voltage Electrostatic Spraying 40-80kv;
Storage Condition: at About 25 Degree and at Ventilated Indoors;
Resistance to Salt Apray: 500HS;
Resistance to Heat and Humidity: 1000h;
Impact Resiatance: 50kg/Cm;
Flexing Endurance: 2mm;
Bulge: 6mm;
|
Color: Red;
Appearance: Powder;
Main Raw Material: Epoxy;
Method: Spray;
Level: Finish Coat;
Drying Method: Drying;
Substrate: Steel;
Components: Pigment;
Formation Mechanism: Conversion Type;
Production Name: Shiny Red Chrome Effect Matel Finished Powader Coa;
Gloss: High Glossy;
Ratio: Spray Ratio Is 90%;
Specific Gravity: 1.2-1.7g Per Cubic Meter;
Storage Stability: Dry, Clean Room;
Application Voltage: 60-90 Kv;
Weight: 25kg/Carton;
Thickness: 60-80um;
Glossy: 90-110%;
Adhesion: 0 Grade;
Hardness: 2h;
Expiration: 12 Months;
Anti Corrition: 500h;
Package: 25kg/Carton;
Storage Condition: at About 25 Degree and at Ventilated Indoors;
|